fig10

Figure 10. Temperature dependence of yield strengths of designed Co-V-Ta-based alloys (CVT, CVTT and CVTA)[17]. For comparison, the yield strengths of the traditional Co- and commercial Ni-based superalloys and newly developed Co-based alloys are plotted in (A) and (B). The alloys were homogenized at 1100 °C for 24 h before annealing.