fig12

Figure 12. (A) FEs of COF-366-Co@CNT, COF-366-(OMe)2-Co@CNT, COF-366-(OH)2-Co@CNT, and COF-366-(F)4-Co@CNT at a scan rate of 5 mV s-1. Copyright 2020, American Chemical Society[145]. (B) LSV curves of NiPc-COF in CO2-saturated and N2-saturated 0.5 m KHCO3 electrolytes at a scan rate of 10 mV S-1. (C) FECO and FEH2 from -0.6 to -1.1 V of NiPc-COF in CO2-saturated 0.5 m KHCO3 electrolytes. Copyright 2020, John Wiley and Sons[146]. (D) Proposed schematic mechanism for electrocatalytic CO2RR on 2D-Co-COF500. (E) PDOS before COOH adsorbed on 2D-Co-COF500. (F) PDOS before COOH adsorbed on Co-COF500. Copyright, 2022 Elsevier[147].