fig9

Figure 9. (A-C) SEM images of CMK-3/SeS2@PDA, CMK-3/SeS2@PDA, and (D) CMK-3/SeS2 were disassembled, and their corresponding cathode electrode films were taken out and immersed in DOL solvent for 2 h, (E) Comparison of cycle performance between CMK-3/SeS2 and CMK-3/SeS2@PDA at a current density of 0.2 A g-1, (F) Rate performance at various current densities from 0.2 to 5 A g-1 of CMK-3/SeS2@PDA, (G) Prolonged cycle life of CMK-3/SeS2@PDA at a current density of 2 A g-1[48], Copyright 2017, Wiley-VCH. (H) Schematic diagram of the discharge-charge process of S8/NMC and SenS8-n/NMC, (I) Schematic model of the